| Group A | Group B |
|---|---|
| P: Hot tears | 1: Improper fusion of two streams of liquid metal |
| Q: Shrinkage | 2: Low permeability of the sand mould |
| R: Blow holes | 3: Volumetric contraction both in liquid and solid stage |
| S: Cold shut | 4: Differential cooling rate |
Choose one answer to reveal the solution.
This is a 2-question preview. The full 2-question timed test opens after free signup.
What visitors can use on this page
The preview questions and their step-by-step solutions are public. The full casting defects test, saved progress, performance reports, Maya AI chat, friend battles and the personalised plan open the signup modal.
GATE ME Casting Defects practice FAQ
Can I solve these GATE ME Casting Defects questions for free?
Yes. The preview questions, answers and step-by-step solutions on this page are free to read without any login.
What opens after free signup?
Signup unlocks the full GATE ME Casting Defects topic test, saved attempts, performance analysis, Maya AI doubt-chat, friend challenges and a personalised study plan.
Are the solutions explained step by step?
Yes. Every question here carries a worked solution so you understand the method, not just the final answer.